Microstructure, interface characteristics and tribological properties of laser cladded NiCrBSi-WC coatings on PH 13-8 Mo steel
Affiliation auteurs | !!!! Error affiliation !!!! |
Titre | Microstructure, interface characteristics and tribological properties of laser cladded NiCrBSi-WC coatings on PH 13-8 Mo steel |
Type de publication | Journal Article |
Year of Publication | 2021 |
Auteurs | Yan X, Chang C, Deng Z, Lu B, Chu Q, Chen X, Ma W, Liao H, Liu M |
Journal | TRIBOLOGY INTERNATIONAL |
Volume | 157 |
Pagination | 106873 |
Date Published | MAY |
Type of Article | Article |
ISSN | 0301-679X |
Mots-clés | Interface characteristics, Laser cladding, microstructural evolution, NiCrBSi-WC coating, Tribological properties |
Résumé | Multiple NiCrBSi-WC coatings with good macro morphology and uniform microstructure were manufactured on PH 13-8Mo steel substrate using laser cladding (LC) technology. Microstructure, interface characteristics and tribological properties of the laser cladded NiCrBSi-WC coatings were researched utilizing optical microscope (OM), X-ray diffraction (XRD), and scanning electron microscopy (SEM) equipped with an energy-dispersive X-ray spectroscopy (EDS) unit. In XRD pattern of the NiCrBSi-WC coatings, gamma-(Ni, Fe) solid solutions with numerous secondary carbides and intermetallic compounds can be found including W2C, Ni3B, and M23C6. Cooling rate of this LC process can be determined as 1.5 x 10(6) K/s. Ultra-high hardness secondary carbides evenly distributed in the fine gamma-(Ni, Fe) columnar dendrites can be observed in the coatings. From top of the coatings to the substrate, the averaged microhardness of the coatings, dilution area, heat-affected zone and substrate is 1008 +/- 48.2 HV0.2, 842 +/- 31.8 HV0.2, 386 +/- 24.4 HV0.2, 356 +/- 3.0 HV0.2, respectively. The coatings presented the best tribological properties with the lowest average coefficient of friction (COF = 0.28) and the wear rate (3.92 +/- 0.72 x 10(-6) mm(3)/(N.m)). A step feature can be observed in the dynamic stable wear process of the interface at the coating/substrate. Good tribological performances of the interface at the coating/substrate with low average COF (0.40) and wear rate (31.83 +/- 2.12 x 10(-6) mm(3)/(N.m)) can be obtained. |
DOI | 10.1016/j.triboint.2021.106873 |